Textile Combing 100 Questions(2)Issuing time:2022-05-04 11:00 How to configure the production process of comber spinning Xinjiang long-staple cotton, especially American Pima cotton?Answer: If the low noil can take into account the quality requirements of the household, the forward feeding process should be adopted as much as possible. In addition, a short de-feeding length can be configured, and the quantification of small rolls can be selected within the range of 70-72g/m. Familiar with the selfcleaning function of laps, if the quality requirements of consumers are high, the back feeding method and a very large extraction distance can be used to greatly improve the combing noil rate. Hazard, the design of the short roller grab is 1-2mm larger than the normal design. Suzhou Yuedaer Textile Brush,combing brush,Circular brushes,industrial brush,strip brushes 02 How to solve the high knot of combed cotton? Answer: The preventive measures to solve the excessive neps of the combed sliver have the following aspects: 1. Select the appropriate type and specification of needle teeth, preferably a zigzag overall cylinder, to maintain the condition of the card clothing for a long time from beginning to end, and to improve carding and impurity removal. 2. Check whether the production process enters the car and whether the production process is appropriate, such as the precise positioning of the bow plate, the high and low entry and exit of the top comb, 3. Properly increase the noil spacing, increase the noil rate, and improve the elimination. 4. Overhaul or disassemble the soft brush, correct the insertion of the soft brush into the deep level of the cylinder, and adjust the speed of the soft brush. 5. Reduce the length of cotton feeding, appropriately reduce the weight of small rolls, reduce the carding load of the cylinder top comb, and ensure the carding quality. 6. If the preparation of the small rolls is poor, the straightness, flatness and separation of the synthetic fibers are not high, and the arrangement of the synthetic fibers in the small rolls is disordered or sticky rolls are likely to cause neps. Therefore, the quality of small rolls should be improved. 03 What is the reason for the broken edge of the cotton net in the comber? What are the preventive measures? Comber brush Comber PB33 round brush 1.jpg Answer: The broken edge of the cotton net of the comber is a relatively wide range of difficulties. The reasons for this are related to various factors such as the condition of the combing machine, the basic parameters of the production process, the airflow configuration, the raw materials, and the temperature and humidity. Over the years, everyone has conducted many tracking analysis experiments on this difficulty and found some preventive measures to solve the problem. The following are summarized. (1) Reasonable setting of small volume quantitative and cotton feeding length. Social experience, the small volume is too light, the length of the cotton is too large, and it is easy to cause the edge of the cotton net to be broken. The cJ 14.5 tex yarn is strongly recommended to use a small volume of 65g/m or more; cJ 11.7 tex, cJ 9.7 tex yarn can use a 63g/m or so. The daily cotton feeding length of 4.7 mm should be used as far as possible. (2) Set the speed reasonably. After the speed of the comber is increased, the output cotton web is affected by the reciprocating traction rope, which is obvious when the lower gear is swayed. In addition, the increase of the speed of the comber leads to an increase in the frictional resistance, and the brush of the comber makes the outer sides of the nipper shaft to synthesize. The fibers are inclined outward in an "eight" shape, resulting in a decrease in the length of the gap connection on both sides of the cotton web. When spinning Xinjiang long-staple cotton, the long and thin beginning end is easy to relax, and the position where it touches the surface of the extraction roller is lower when it is slowly extracted. , it is also more prone to side hooks. Therefore, choose Xinjiang long-staple cotton and middle-Xinjiang long-staple cotton to spin fine yarn. When the weight is relatively light, the speed should be reduced as much as possible, and it is recommended to be around 250 clamp times/min. Comber brush (3) Adjust the airflow. When the edge of the cotton net is broken, the damage of the airflow in the long air duct should be fully considered at first, and the mouth opening specification of the rear triangle airflow plate of the vehicle body should be adjusted. Pay special attention to the damage of the airflow on both sides. (4) Improve the edge forming of small rolls. The poor edge of the small roll is one of the reasons for the broken edge. Attention should be paid to adjusting the uniformity of the cotton roll made by the fully prepared mechanical equipment, especially the cotton layer on the edge of the small roll should be uniform and tidy, which is beneficial to the nipper grasping and combing. Keep the thickness of the cotton layer uniform throughout the process. (5) Adjustment of the adjustable cotton device. When using a dispatchable cotton device, the specifications of the opening mouth of the cotton collector can be adjusted according to the input of the cotton web to the cotton roller, and the position of the cotton collector can not be higher than the surface of the extraction roller. And ensure that the cotton layer does not touch the edge of the collecting block when entering. Adjust its position as much as possible to avoid contact between synthetic fibers and parts. (6) Pay attention to the condition of the extraction glue stick. When there is a broken edge on one side of the cotton mesh, check whether the punching on both sides of the extraction glue stick is consistent, check whether the air film in the punching arm is damaged, and disassemble it immediately if necessary. When the surface condition of the extraction glue stick is poor and sticking often occurs, it should be cleaned or regrinded immediately, and industrial coating treatment should be carried out. Comber brush (7) Adjust raw materials and control temperature and humidity. When edge breakage is common, one should consider the damage to the cohesion of the cotton web caused by the raw material or pre-spinning production and processing of short staples, and adjust all aspects of the raw material or pre-spinning production process when necessary. If the raw cotton sugar content is high, attention should also be paid to the cleaning of the shaft of the nipper, the surface of the extraction roller, both sides of the cotton collector and the side of the cotton passing plate. The second is to fully consider the damage caused by the temperature and humidity of the production line. The temperature and humidity should be reasonably monitored according to different seasons. According to the work experience, a more reasonable relative air humidity is 55%, and a more reasonable temperature is 24 ℃ ~ 25 ℃. (8) Select the cotton guide method. In order to reduce edge breakage, it is advisable to use a closed-type small cotton guide plate to increase the edge-closing angle as much as possible. 04 Why is the amount of noil fed backwards larger than that fed forwards? Comber brush Answer: If the noil spacing is 16mm and the feeding amount is 5.2mm, the fiber length of the noil fed forward is likely to be 11.8 (16-5.2) mm, and the backward feeding is likely to become noil The fiber length of cotton is 21.2 (16 5.2) mm. It is known from the above that the length of the cotton noil is longer than that of the forward feeding, and the noil rate is larger. 05 The situation of combed unwinding and sticking is serious, why is it like that? Answer: There are several reasons why the small roll sticks to the roll: Needle comb round brush-(2).jpg 1. Raw cotton has high short staple content; 2. Poor carding quality (single fiberization level) cleaning production process leads to short piles; 3. The number of mergings and understretching ratios of the fully prepared production process is not properly selected, and it is necessary to reduce merging, small understretching, and prevent rotten rolls; 4. The punching of small rolls is too large, and the beta ray machine and equipment in the disk are poor (the strip roll or parallel roll degumming machine and equipment and the improvement of the gradual pressing machine and equipment); 5. The lap unwinding capacity of the comber is large, and the bearing capacity should be controlled too small. The unwinding rollers on both sides land, and the unwinding method is "changed from the surface to the line" to ensure the expected effect of unwinding; 6. The overlapping feeding of the feeding sliver that is prepared for the full production process should be closely connected with the vertical surface feeding, expanding and cohesion, to prevent stratification; 7. Combing and preparation are not good enough to control the temperature, environment and humidity of the production process. 06 When spinning Xinjiang long-staple cotton for 80s, when the speed of E65 is more than 400 nips/min, there are serious edge breakage and cloud spots. How to adjust the production process to solve this problem? Comber brush Answer: There are many factors that damage the quality of the cotton web. It should be adjusted comprehensively from the past to the back: at the beginning, adjust the edge of the small roll to ensure the high quality of the small roll structure, and adjust the negative working pressure of the comber noil noil without sticking and breaking the edge. High, the output cotton layer of the combed cotton web is not easy to be too thin, and the quantitative improvement of small rolls can be improved. Changing to forward feeding can also improve lap breakage. Rational formulation of extraction roller shunting If the restart is too late or the soft brush speed is too high, it is easy to cause cloud spots on the cotton net. Suzhou Yuedaer Textile Brush,combing brush,Circular brushes,industrial brush,strip brushes |